This sample was monodisperse.
Au was deposited at a 30 degree angle to 15 nm thickness.
Colloidal gold particles were deposited by dipping into dilute solution.
The specimen was frozen at high pressure using the bal-tec hpm 010 instrument.
The embedded sample was sectioned at 100 K to 50 nm final thickness.